Mesophase pitches, precursors of high-performance carbon fibers, were prepared from petroleum pitch by a two-stage heat treatment, in a reactor capable of heat treating 700 g of petroleum pitch under stirring. The process consisted of a pretreatment under pressure at 390, 410 and 430 °C under nitrogen atmosphere, at 0.9 MPa, for three hours, as the first stage, followed by another heat treatment under atmospheric pressure, as the second stage. To study the properties of the petroleum pitch samples, during the experiment, they were removed from the system. Quinoline insolubles, toluene insolubles, mesophase content and softening point of the samples were used to follow the pyrolysis process. The results revealed slight variations in the properties for the pitches produced at 390 and 410 °C. However, the pitch samples produced at 430 °C had softening points higher than 300 °C, and mesophase contents of around 70%.

Petroleum pitch; pyrolysis; mesophase pitch


Associação Brasileira de Polímeros Rua São Paulo, 994, Caixa postal 490, São Carlos-SP, Tel./Fax: +55 16 3374-3949 - São Carlos - SP - Brazil
E-mail: revista@abpol.org.br